Low-Damage Stripping for 60–80 μm Polarization-Maintaining Fiber

Application Challenge

Preserve fragile small-diameter PM fiber during coating removal, where excessive force or uncontrolled stripping can compromise handling and downstream performance.

Recommended Workflow

Secure the fiber with appropriate support, remove the coating using a low-damage stripping method, inspect the bare fiber, then cleave and splice under controlled alignment conditions.

Process Controls

  • Low mechanical stress on 60–80 μm fiber
  • Controlled stripping length and support geometry
  • Preparation suitable for precision PM-fiber workflows

Recommended Equipment

VAEYI precision stripping tools and accessories configured for delicate specialty-fiber preparation.

Tell Us About Your Fiber and Process.

Share the fiber specifications, processing result and tool or equipment purchase quantity for your application.

Your Fiber

Fiber type, cladding and coating diameters, and coating material, if known.

Your Process

Stripping, cleaving or splicing, and the processing result you need.

Your Purchase Quantity

Number of tools or equipment units, sample needs or estimated order quantity.

Not sure about every detail? Send the information you have.

Discuss Your Requirements